Ibhloko yeKhabhoni yeCathode
Iinkcukacha ezikhawulezayo:
Igama lemveliso:Ibhloko yekhabhoni yeCathode
Igama lebrand:QF
Ukuxhathisa (μΩ.m):9-29
Ubuninzi obubonakalayo (g/cm³):1.60-1.72
Amandla okuGuquka (N/㎡):8-12
Umbala:Mnyama
Izixhobo:i-petroleum coke kunye ne-needle coke ekumgangatho ophezulu
Ubungakanani:njengemfuneko yomthengi
Isicelo:I-aluminium ye-electrolytic
uxinano lokwenyani:1.96-2.20
Uthuthu:0.3-2
ukwandiswa kwe-sodium:0.4-0.7
Inkcazo yokuPakisha:Ukupakisha ngeebhokisi zomthi kunye nebhanti yentsimbi.
Inkcazo
| Iinkcukacha | Iyunithi | Indlela yovavanyo | Ixabiso | |||
| I-30%GraphiteAddad | I-50% yeGraphite yongeziwe | Ibanga leGraphitic | Ibanga leGraphitized | |||
| Uxinano Lwenene | g/cm | I-ISO21687 | ≥1.98 | ≥1.98 | ≥2.12 | ≥2.20 |
| Uxinano olubonakalayo | g/cm | I-ISO12985.1 | ≥1.60 | ≥1.60 | ≥1.62 | ≥1.62 |
| I-Porosity evulekileyo | % | I-ISO12985.2 | ≤16 | ≤16 | ≤18 | ≤20 |
| I-Porosity iyonke | % | ≤19 | ≤19 | ≤23 | ≤27 | |
| Amandla Okucinezela (okanye Amandla Okutyumza Okubandayo) | I-MPa | I-ISO18515 | ≥26 | ≥26 | ≥26 | ≥20 |
| Amandla okuGuquka | I-MPa | IS012986.1 | ≥7 | ≥7 | ≥7 | ≥7 |
| Ukumelana ngqo kombane | uom | I-ISO11713 | ≤35 | ≤30 | ≤21 | ≤12 |
| Ukuqhuba kweThermal | W/mk | IS012987 | ≥13 | ≥15 | ≥25 | ≥100 |
| I-Coefficient yoLwandiso lweThermal oluLungelelanisiweyo | 106/K | I-ISO14420 | ≤4.0 | ≤4.0 | ≤4.0 | ≤3.5 |
| Umxholo wothuthu | % | I-ISO8005 | ≤5 | ≤3.5 | ≤1.5 | ≤0.5 |
| Ukwandiswa kweSodium (okanye ukudumba kweRapoport okanye ukudumba yiAlkali) | % | I-ISO15379.1 | ≤0.8 | ≤0.7 | ≤0.5 | ≤0.4 |